Search

tensile yield strength of group 4 elements

Input interpretation

group 4 elements | tensile yield strength
group 4 elements | tensile yield strength

Results

titanium | 140 MPa (megapascals) zirconium | 230 MPa (megapascals) hafnium | (data not available) rutherfordium | (data not available)
titanium | 140 MPa (megapascals) zirconium | 230 MPa (megapascals) hafnium | (data not available) rutherfordium | (data not available)
group 4 elements | tensile yield strength | 185 MPa (megapascals) (median) (based on 2 values; 2 unavailable)
group 4 elements | tensile yield strength | 185 MPa (megapascals) (median) (based on 2 values; 2 unavailable)

Ranked values

 | visual | ratios | | comparisons titanium | | 0.61 | 1 | 39% smaller zirconium | | 1 | 1.64 | 64% larger
| visual | ratios | | comparisons titanium | | 0.61 | 1 | 39% smaller zirconium | | 1 | 1.64 | 64% larger

Unit conversions for median tensile yield strength 185 MPa

0.185 GPa (gigapascals)
0.185 GPa (gigapascals)
1.85×10^8 Pa (pascals)
1.85×10^8 Pa (pascals)
1.85×10^8 N/m^2 (newtons per square meter)
1.85×10^8 N/m^2 (newtons per square meter)
1830 atm (atmospheres)  (unit officially deprecated)
1830 atm (atmospheres) (unit officially deprecated)
26800 psi (pounds-force per square inch)
26800 psi (pounds-force per square inch)

Comparison for median tensile yield strength 185 MPa

 ≈ ( 0.002 ≈ 1/540 ) × theoretical tensile strength of a carbon nanotube ( ≈ 100 GPa )
≈ ( 0.002 ≈ 1/540 ) × theoretical tensile strength of a carbon nanotube ( ≈ 100 GPa )