ferromagnetic elements | phase at STP
Results
cobalt | solid gadolinium | solid iron | solid nickel | solid
ferromagnetic elements | phase at STP | solid | solid | solid | solid (all)
Thermodynamic properties
phase at STP | all | solid melting point | median | 1475 °C | highest | 1538 °C (iron) | lowest | 1313 °C (gadolinium) | distribution | boiling point | median | 2920 °C | highest | 3250 °C (gadolinium) | lowest | 2861 °C (iron) | distribution | molar heat of fusion | median | 15 kJ/mol | highest | 17.2 kJ/mol (nickel) | lowest | 10 kJ/mol (gadolinium) | distribution | molar heat of vaporization | median | 361 kJ/mol | highest | 378 kJ/mol (nickel) | lowest | 305 kJ/mol (gadolinium) | distribution | specific heat at STP | median | 433 J/(kg K) | highest | 449 J/(kg K) (iron) | lowest | 240 J/(kg K) (gadolinium) (properties at standard conditions)