semiconductors | molar magnetic susceptibility
Results
![germanium | -1.09×10^-10 m^3/mol (cubic meters per mole) silicon | -4.49×10^-11 m^3/mol (cubic meters per mole) tellurium | -4.98×10^-10 m^3/mol (cubic meters per mole)](../image_source/add2aa247cdacb832a5ead38c2c18021.png)
germanium | -1.09×10^-10 m^3/mol (cubic meters per mole) silicon | -4.49×10^-11 m^3/mol (cubic meters per mole) tellurium | -4.98×10^-10 m^3/mol (cubic meters per mole)
![semiconductors | molar magnetic susceptibility | -1.09×10^-10 m^3/mol (cubic meters per mole) (median)](../image_source/c3b5d9e95b045631490073ff4d98134e.png)
semiconductors | molar magnetic susceptibility | -1.09×10^-10 m^3/mol (cubic meters per mole) (median)
Unit conversions for median molar magnetic susceptibility -1.09×10^-10 m^3/mol
![-0.109 mm^3/mol (cubic millimeters per mole)](../image_source/c2f3485427b25bbeb91c5965c20bf11a.png)
-0.109 mm^3/mol (cubic millimeters per mole)
![-1.09×10^-4 cm^3/mol (cubic centimeters per mole)](../image_source/2030492bc8b31469402d0e094be0d465.png)
-1.09×10^-4 cm^3/mol (cubic centimeters per mole)