Search

bulk modulus of actinides

Input interpretation

actinides | bulk modulus
actinides | bulk modulus

Bulk modulus rankings

1 | thorium | 54 GPa 2 | uranium | 100 GPa (based on 2 values; 13 unavailable)
1 | thorium | 54 GPa 2 | uranium | 100 GPa (based on 2 values; 13 unavailable)

Unit conversions for median bulk modulus 77 GPa

0.077 TPa (terapascals)
0.077 TPa (terapascals)
7.7×10^10 Pa (pascals)
7.7×10^10 Pa (pascals)
7.7×10^10 N/m^2 (newtons per square meter)
7.7×10^10 N/m^2 (newtons per square meter)
760000 atm (atmospheres)  (unit officially deprecated)
760000 atm (atmospheres) (unit officially deprecated)

Comparisons for median bulk modulus 77 GPa

 ≈ 0.35 × gold bulk modulus ( ≈ 220 GPa )
≈ 0.35 × gold bulk modulus ( ≈ 220 GPa )
 ≈ 0.45 × iron bulk modulus ( ≈ 170 GPa )
≈ 0.45 × iron bulk modulus ( ≈ 170 GPa )
 ≈ 2.3 × carbon bulk modulus ( ≈ 33 GPa )
≈ 2.3 × carbon bulk modulus ( ≈ 33 GPa )

Corresponding quantity

Compressibility β from β = 1/K:  | 1.3×10^-11 Pa^(-1) (reciprocal pascals)
Compressibility β from β = 1/K: | 1.3×10^-11 Pa^(-1) (reciprocal pascals)