Input interpretation

lanthanides | phase at STP
lanthanides | phase at STP

Summary

solid
solid

Table

lanthanum | solid cerium | solid praseodymium | solid neodymium | solid promethium | solid samarium | solid europium | solid gadolinium | solid terbium | solid dysprosium | solid holmium | solid erbium | solid thulium | solid ytterbium | solid lutetium | solid
lanthanum | solid cerium | solid praseodymium | solid neodymium | solid promethium | solid samarium | solid europium | solid gadolinium | solid terbium | solid dysprosium | solid holmium | solid erbium | solid thulium | solid ytterbium | solid lutetium | solid

Thermodynamic properties

phase at STP | all | solid melting point | median | 1100 °C  | highest | 1663 °C (lutetium)  | lowest | 798 °C (cerium)  | distribution |  boiling point | median | 3000 °C  | highest | 3464 °C (lanthanum)  | lowest | 1196 °C (ytterbium)  | distribution |  molar heat of fusion | median | 9.2 kJ/mol  | highest | 22 kJ/mol (lutetium)  | lowest | 5.5 kJ/mol (cerium)  | distribution |  molar heat of vaporization | median | 285 kJ/mol  | highest | 415 kJ/mol (lutetium)  | lowest | 160 kJ/mol (ytterbium)  | distribution |  specific heat at STP | median | 182 J/(kg K)  | highest | 240 J/(kg K) (gadolinium)  | lowest | 154 J/(kg K) (ytterbium and lutetium)  | distribution |  Néel point | median | 90.5 K  | highest | 230 K (terbium)  | lowest | 12.5 K (cerium)  | distribution |  (properties at standard conditions)
phase at STP | all | solid melting point | median | 1100 °C | highest | 1663 °C (lutetium) | lowest | 798 °C (cerium) | distribution | boiling point | median | 3000 °C | highest | 3464 °C (lanthanum) | lowest | 1196 °C (ytterbium) | distribution | molar heat of fusion | median | 9.2 kJ/mol | highest | 22 kJ/mol (lutetium) | lowest | 5.5 kJ/mol (cerium) | distribution | molar heat of vaporization | median | 285 kJ/mol | highest | 415 kJ/mol (lutetium) | lowest | 160 kJ/mol (ytterbium) | distribution | specific heat at STP | median | 182 J/(kg K) | highest | 240 J/(kg K) (gadolinium) | lowest | 154 J/(kg K) (ytterbium and lutetium) | distribution | Néel point | median | 90.5 K | highest | 230 K (terbium) | lowest | 12.5 K (cerium) | distribution | (properties at standard conditions)