Search

resistivity of platinum

Input interpretation

platinum | resistivity
platinum | resistivity

Result

1.1×10^-7 Ω m (ohm meters)
1.1×10^-7 Ω m (ohm meters)

Unit conversions

11 μΩ cm (microohm centimeters)
11 μΩ cm (microohm centimeters)
110 nΩ m (nanoohm meters)
110 nΩ m (nanoohm meters)
0.11 μΩ m (microohm meters)
0.11 μΩ m (microohm meters)
1.1×10^-5 Ω cm (ohm centimeters)
1.1×10^-5 Ω cm (ohm centimeters)
4.3×10^-6 Ω in (ohm inches)
4.3×10^-6 Ω in (ohm inches)
11000 emus  (unit officially deprecated)
11000 emus (unit officially deprecated)
1.2×10^-17 esus  (unit officially deprecated)
1.2×10^-17 esus (unit officially deprecated)
1.2×10^-17 statΩ cm (statohm centimeters)  (unit officially deprecated)
1.2×10^-17 statΩ cm (statohm centimeters) (unit officially deprecated)
0.51 atomic units
0.51 atomic units

Comparisons as electric resistivity

 ≈ resistivity of tin at 20 °C ( ≈ 1×10^-7 Ω m )
≈ resistivity of tin at 20 °C ( ≈ 1×10^-7 Ω m )
 ≈ 1.1 × resistivity of iron at 20 °C ( ≈ 9.7×10^-8 Ω m )
≈ 1.1 × resistivity of iron at 20 °C ( ≈ 9.7×10^-8 Ω m )
 ≈ resistivity of gold at 1000 K ( ≈ 9×10^-8 Ω m )
≈ resistivity of gold at 1000 K ( ≈ 9×10^-8 Ω m )

Corresponding quantity

Conductivity σ from σ = 1/ρ:  | 9.1×10^6 S/m (siemens per meter)